dark gray powder(s), a=0.2817nm, c=1.4059 nm; can be prepared by reacting Li2CO3 or LiOH·H2O with CoCO3 at 850°C–900°C for 24 h in air; used in ceramics and as an insertion electrode in Li battery systems; has fluxing properties of lithium oxide, and enhances adhesion similar to cobalt oxide [HAW93] [STR93] [DAH90] [GUM92]
Uses
Lithium cobalt(III) oxide is a critical substance in the quest for high performance, advanced batteries. It is used as a lithium ion cathode material.
Uses
Critical substance in the quest for high performance, advanced batteries.1
General Description
This product has been enhanced for energy efficiency.
Flammability and Explosibility
Notclassified
LITHIUM COBALT(III) OXIDE Preparation Products And Raw materials